光谱学与光谱分析 |
|
|
|
|
|
Topography Structure and Flocculation Mechanism of Polymeric Phosphate Ferric Sulfate(PPFS) |
ZHENG Huai-li1, ZHANG Hui-qin1, JIANG Shao-jie1, LI Fang2, JIAO Shi-jun1, FANG Hui-li1 |
1. Key Laboratory of the Three Gorges Reservoir Regions Eco-Environment, Ministry of Education, Chongqing University, Chongqing 400045, China 2. College of Chemistry, Sichuan University, Chengdu 610064, China |
|
|
Abstract Characteristics of polymeric phosphate ferric sulfate (PPFS) were investigated using FTIR (Fourier transform infrared spectrometer), XRD (X-ray diffraction) and SEM (scanning electron microscope) in the present study. The formed PPFS structure and morphology were stereo meshwork, which was clustered and close to coral reef, synthesis of high charge density, bioactive polyhydroxy and mixed polynuclear complex PPFS. The results showed that charge neutralization of PPFS had not played a decisive role in the coagulation beaker test and the zeta potential proved that PPFS was largely affected by bridging and netting sweep. Therefore, the coagulation mechanisms of PPFS were mainly composed of charge neutralization, adsorption bridging and netting sweep mechanisms.
|
Received: 2010-07-13
Accepted: 2010-10-23
|
|
Corresponding Authors:
ZHENG Huai-li
E-mail: zhl@cqu.edu.cn
|
|
[1] LI Feng-ting(李风亭). Industrial Water Treatment (工业水处理), 2002, 22(1): 5. [2] Jordan Jacqueline A, Verhoff Ashley M, Morgan Julie E, et al. In Vitro Cellular & Developmental Biology-Animal, 2009, 45(10): 602. [3] Lei G Y, Ma J, Guan X H, et al. Desalination, 2009, 247(1-3): 518. [4] Liang Z, Wang Y X, Zhou Y, et al. Water Science and Technology, 2009, 59(6): 1129. [5] Voegelin A, Kaegi R, Frommer J, et al. Geochimicaet Cosmochimica Acta, 2010, 74(1): 164. [6] Wei J C, Gao B Y, Yue Q Y, et al. Journal of Hazardous Materials, 2009, 165(1-3): 789. [7] DAI Jun, LEI Hong-ying, SUN Jian-qi, et al(代 军, 雷红英, 孙剑奇, 等). Mining and Gandmetallurgical Engineering(矿冶工程), 2008, 28(6): 41, 47. [8] Gregory J. Journal of Environmental Sciences-China, 2009, 21(1): 2. [9] XU Hao-long, WANG Chang-zhi, ZHANG Yi-dan(徐灏龙, 王长智, 章一丹). Water & Wastewater Engineering (给水排水), 2009, 35: 319. [10] YU Hui, ZHU Yin-hua, LIU Chang, et al(于 荟, 朱银华, 刘 畅, 等). Chinese Journal of Catalysis (催化学报), 2009, 30(3): 265. [11] JIANG Fang, ZHENG Zheng, ZHENG Shou-rong, et al(江 芳, 郑 正, 郑寿荣, 等). Environmental Chemistry(环境化学), 2008, 27(5): 565. [12] SHI Zhen-rong, CAI Ke-qin (石振荣, 蔡克勤). Acta Petrologica Et Mineralogica (岩石矿物学杂志), 2008, 27(2): 164. [13] Jiao S J, Zheng H L, Chen R, et al. Journal of Central South University of Technology, 2009, 16(s1): 345. [14] LIU Hong, SHAO Jun, LIANG Jing, et al(刘 红, 邵 俊, 梁 晶, 等). Chinese Journal of Environmental Engineering (环境工程学报), 2008, 2(4): 476.
|
[1] |
TANG Gu-hua, ZHANG Hui, SUN Xin-yuan, XU Meng, OUYANG Jian-ming*. Differences in Adsorption of Anionic Surfactant AOT by Calcium Oxalate Dihydrate With Different Morphologies[J]. SPECTROSCOPY AND SPECTRAL ANALYSIS, 2021, 41(04): 1079-1085. |
[2] |
LIN Jia-wei, LI Jie*, WU Jing-xuan, LI Min, ZHANG Wen-hao. Influence Mechanism and Analysis of Infrared Spectrum of NH+4 and F- on Fluorite Flotation[J]. SPECTROSCOPY AND SPECTRAL ANALYSIS, 2021, 41(04): 1281-1287. |
[3] |
LI Jun-jun, HOU Shan-hua, XIA Zhi-yue, OUYANG Jian-ming*. The Property Changes of Urine Crystallites of Calcium Oxalate Stone Formers before and after Taking Medicine[J]. SPECTROSCOPY AND SPECTRAL ANALYSIS, 2011, 31(08): 2263-2267. |
[4] |
ZHENG Huai-li, JIAO Shi-jun, HE Qiang, CHEN Rong, ZHANG Peng, FANG Hui-li . Study of Ferric Species Distribution in Polymeric Phosphate Ferric Sulfate (PPFS) [J]. SPECTROSCOPY AND SPECTRAL ANALYSIS, 2011, 31(02): 551-554. |
[5] |
YANG Jin, HUANG Zhi-jie, HOU Shan-hua, OUYANG Jian-ming* . Composition Analyses of Urinary Microcrystalline in Urine of Magnesium Ammonium Phosphate Stones Formers and Its Relationship with the Stones Formation [J]. SPECTROSCOPY AND SPECTRAL ANALYSIS, 2011, 31(01): 168-172. |
[6] |
HUANG Zhi-jie, TAN Jin, OUYANG Jian-ming* . Components of Urinary Crystallites in Urine of Uric Acid Stone Formers and Its Relationship with Formation of Stones [J]. SPECTROSCOPY AND SPECTRAL ANALYSIS, 2010, 30(09): 2350-2354. |
[7] |
HUANG Zhi-jie, LI Jun-jun, HE Jie-yu, OUYANG Jian-ming* . Study on Nano- and Microcrystallites in the Urines of Calcium Oxalate Stone Formers [J]. SPECTROSCOPY AND SPECTRAL ANALYSIS, 2010, 30(07): 1913-1917. |
[8] |
ZHANG Ju-hua1, 2, XING Jian-min1*, JIANG Yang-yang1, 2, GAO Hong-shuai1, 2, LIU Hui-zhou1 . Study on the pH-Sensitive Secondary Structure of γ-PGA Embedded with Magnetite Nanoparticles [J]. SPECTROSCOPY AND SPECTRAL ANALYSIS, 2009, 29(08): 2148-2151. |
[9] |
LI Lu-hai1,2,ZHANG Shu-fen1,YANG Jin-zong1,ZOU Jing1,2,ZHAO Qiang2 . Charge Control and IR Analysis of Amine on Diarylide Yellow Pigment PY14 [J]. SPECTROSCOPY AND SPECTRAL ANALYSIS, 2005, 25(10): 1584-1587. |
[10] |
SHEN Yu-hua1, 3, HUANG Fang-zhi1, XIE An-jian1, 3, XIONG Qi-ru2, CHEN Kai-bo1 . Stability of Patient Bile and Study on Its Influential Factors[J]. SPECTROSCOPY AND SPECTRAL ANALYSIS, 2005, 25(10): 1648-1651. |
|
|
|
|